WO2002008835A2 - High-resolution overlay alignment methods and systems for imprint lithography - Google Patents
High-resolution overlay alignment methods and systems for imprint lithography Download PDFInfo
- Publication number
- WO2002008835A2 WO2002008835A2 PCT/US2001/022317 US0122317W WO0208835A2 WO 2002008835 A2 WO2002008835 A2 WO 2002008835A2 US 0122317 W US0122317 W US 0122317W WO 0208835 A2 WO0208835 A2 WO 0208835A2
- Authority
- WO
- WIPO (PCT)
- Prior art keywords
- template
- substrate
- patterned template
- liquid
- substtate
- Prior art date
Abstract
Description
Claims