US20060183410A1 - Diamond conditioning of soft chemical mechanical planarization/polishing (CMP) polishing pads - Google Patents
Diamond conditioning of soft chemical mechanical planarization/polishing (CMP) polishing pads Download PDFInfo
- Publication number
- US20060183410A1 US20060183410A1 US11/402,449 US40244906A US2006183410A1 US 20060183410 A1 US20060183410 A1 US 20060183410A1 US 40244906 A US40244906 A US 40244906A US 2006183410 A1 US2006183410 A1 US 2006183410A1
- Authority
- US
- United States
- Prior art keywords
- polishing pad
- soft polishing
- conditioning
- diamond
- platen
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Abandoned
Abstract
Conditioning of chemical mechanical planarization (CMP) using conventional diamond-embedded abrasive strips are well suited to condition conventional “hard” polishing but not soft polishing pads because the diamonds not only remove waste material, but they also damage the polishing surface of the pad. Embodiments of the present invention condition soft polishing pads using diamond strips without damaging the soft polishing pad.
Description
- The present application is a Divisional of U.S. Ser. No. 10/402,578, filed Mar. 28, 2003.
- 1. Field
- Embodiments of the present invention relate to chemical mechanical planarization/polishing (CMP) and, in particular, to conditioning of CMP polishing pads.
- 2. Discussion of Related Art
- Chemical mechanical planarization/polishing (CMP) is a process technology first developed in the mid-1980s to enable production of integrated circuits on substrates or wafers. CMP processes are used prepare wafers and to fabricate semiconductor devices or structures on the wafers. A CMP process may be used to planarize (i.e., make flat) a semiconductor layer on a wafer, an insulating layer on the semiconductor layer, and a conductive layer on the insulating layer in predetermined patterns.
- A typical CMP system includes a wafer carrier and a platen mounted in a housing. A polishing pad is secured to the platen and the wafer to be polished is secured in the wafer carrier. A typical CMP process operates as follows. The wafer carrier rotates the wafer and/or the platen rotates the polishing pad. Chemical slurry is applied to the surface of the polishing pad and the wafer is brought into contact with the polishing pad and is polished (or planarized). The combination of applying the chemical slurry and the mechanical rotation leads to the term “chemical-mechanical planarization.”
- As the wafer is polished, the chemical slurry and materials removed from the wafer tend to glaze the surface of the polishing pad, making the polishing pad slick and reducing the polishing rate and efficiency. It is thus important that the polishing pad surface be clean and free of surface irregularities. The process of cleaning the polishing pad is sometimes referred to a “conditioning” or “refreshing.”
- One method of conditioning polishing pads is to abrade them with a conventional diamond-embedded abrasive disk or strip. Although conventional diamond-embedded abrasive strips are well suited to condition “hard” polishing pads used for rough polishing, they are not well suited to condition “soft” polishing pads used for fine polishing. When a soft polishing pad is conditioned with a diamond-embedded abrasive disk, the diamonds not only remove waste material, but they also damage the polishing surface of the pad.
- In the drawings, like reference numbers generally indicate identical, functionally similar, and/or structurally equivalent elements. The drawing in which an element first appears is indicated by the leftmost digit(s) in the reference number, in which:
-
FIG. 1 is schematic diagram of a chemical mechanical planarization/polishing (CMP) polishing system according to an embodiment of the present invention; -
FIG. 2 is a flowchart illustrating a process performed by a CMP polishing system in according to embodiments of the present invention; -
FIG. 3 illustrates an example soft polishing pad according to an embodiment of the present invention; -
FIG. 4 illustrates operation of a conditioning arm according to an embodiment of the present invention; and -
FIG. 5 illustrates a diamond conditioner according to an embodiment of the present invention. -
FIG. 1 is schematic diagram of a chemical mechanical planarization (CMP)polishing system 100 according to an embodiment of the present invention. TheCMP polishing system 100 includes ahousing 101, apolishing head 102, acontrol panel 103, aplaten 104, aspindle 105, awafer 106, abase 107, asoft polishing pad 108, aconditioning arm 110, a diamond (or artificial diamond)conditioner 112, aslurry tank 114, a spindle 115, awater tank 116, andelectromechanical equipment 118. Theslurry tank 114 and/or thewater tank 116 may be located in or separate from thehousing 101. Theelectromechanical equipment 118 may include vertical drivers, rotational drivers, controllers, or other equipment generally used to operate arms, motors, and other devices in CMP polishing systems. - The
platen 104 is mounted in thehousing 101 and may be rotated by a motor (not shown) in theelectromechanical equipment 118. Thepolishing head 102 is mounted on thespindle 105 and may be rotated by a motor (not shown) in theelectromechanical equipment 118. Thewafer 106 is mounted with the surface to be polished face down and away from thepolishing head 102. Thesoft polishing pad 108 mounted to the platen using an adhesive. During polishing of thewafer 106, thepolishing head 102 may be rotated in a direction opposite to the rotation of thepolishing pad 108 may be, as shown byarrows polishing head 102 may rotate while theplaten 104 remains stationary. Alternatively still, thepolishing head 102 may be stationary while theplaten 104 rotates. Theslurry tank 114 delivers slurry to the surface of thesoft polishing pad 108 duringwafer 106 polishing. - The
conditioning arm 110 pivots in itsbase 107 when conditioning thesoft polishing pad 108. A motor (not shown) in theelectromechanical equipment 118 may move theconditioning arm 110. Thewater tank 116 may dispense a rinsing solution, such as potable water or de-ionized (DI) water, to the surface of thesoft polishing pad 108 during conditioning of thesoft polishing pad 108. -
FIG. 2 is a flowchart illustrating a process 200 performed by theCMP polishing system 100 according to embodiments of the present invention. A machine-readable medium with machine-readable instructions thereon may be used to cause a processor to perform the process 200. Of course, the process 200 is only an example process and other processes may be used. The example process 200 may be used to remove metal, oxides, glass, silicon, etc. Although the example process 200 is described with reference to wafers, the example process 200 may be used for semiconductors, memory disks, or other suitable objects requiring smoothness, planarity, fine polishing, etc., such as lenses and mirrors. - In a
block 202 thehead 102 holds thewafer 106 and rotates thewafer 106 against thesoft polishing pad 108 as slurry from theslurry tank 114 is applied to the surface of thesoft polishing pad 108 and theplaten 104 applies a force to thewafer 106. In ablock 204, thehead 102 disengages thewafer 106 from contact with thesoft polishing pad 108 and the slurry stops flowing to the surface of thesoft polishing pad 108. - In a
block 206, thesoft polishing pad 108 is conditioned using thediamond conditioner 112. In one embodiment of the present invention, theplaten 104 rotates thesoft polishing pad 108, rising solution from thewater tank 116 rinses thesoft polishing pad 108, e.g., by supplying DI water to the surface of thesoft polishing pad 108, and theconditioning arm 110 with thediamond conditioner 112 sweeps across (e.g., back and forth) thesoft polishing pad 108. Although polishing of thesoft polishing pad 108 may be described in some embodiments as being performed ex situ (betweenwafer 106 polishings), polishing of thesoft pat 108 in other embodiments may be performed in situ (whilewafers 106 are being polished), or some combination of both. Of course, thesoft polishing pad 108 may be conditioned according to embodiments of the present invention prior to polishing anywafers 106. - One or a combination of the following process parameters may be modified to improve the process for
soft pad 108 conditioning using thediamond conditioner 112 to ensure that theconditioning arm 110 with thediamond conditioner 112 do not destroy or significantly reduce the lifetime of thesoft polishing pad 108. In fact, according to embodiments of the present invention, the lifetime of thesoft polishing pad 108 is significantly increased. Increasedsoft polishing pad 108 lifetime results in reduced labor costs and costs of parts, as well as improved processes, (e.g.,soft polishing pads 108 do not have to be changed as often). - In one embodiment, the
conditioning arm 110 applies approximately 0.25 psi to thesoft polishing pad 108 through thediamond conditioner 112 as opposed to approximately three psi applied using conventional hard polishing pad techniques. - In known soft polishing pad conditioning methods, the platen and thus the soft polishing pad does not rotate. In embodiments of the present invention, the rotational speed of the
platen 104 and thus thesoft polishing pad 108 may be approximately one hundred revolutions per minute 100 (rpm) - In known soft polishing pad conditioning methods, there may be no DI water flowing to the soft conditioning pad. In one embodiment of the present invention, the volumetric flow rate of DI water from the
DI water tank 116 may may be one gallon per minute (gpm). Alternatively, the volumetric flow rate may be anywhere from zero to approximately seven gallons per minute. - In known soft polishing pad conditioning methods, there is no diamond conditioner used, thus no down force applied to a soft polishing pad In one embodiment, the down force applied to the soft polishing pad by the
diamond conditioner 112 may be 0.25 psi. - In known soft polishing pad conditioning methods, no diamond conditioner is used. n known hard polishing pad conditioning methods, the diamond conditioner makes at least ten sweeps. In one embodiment, the
diamond conditioner 112 makes one sweep across the soft polishing pad. -
FIG. 3 illustrates the examplesoft polishing pad 108 according to an embodiment of the present invention. The examplesoft polishing pad 108 includes several pores 302 and may be made from napped poromerics-porous urethane layers on a mylar or compressible urethane substrate. In an alternative embodiment, the examplesoft polishing pad 108 may be a soft pad made with tangled polyester fibers coated with polyurethane. In another embodiment, the examplesoft polishing pad 108 may be a felt sheet of fibers impregnated with micro porous elastomer. Alternatively still, the examplesoft polishing pad 108 may be a porous thermoplastic resin matrix, typically polyurethane, reinforced with a fibrous network such as a felted mat of polyester fibers. An example of a suitable soft pad includes any of the Politex® Series polishing pads available from Rodel Holdings in Wilmington, Del. - The
soft polishing pads 108 according to embodiments of the present invention are to be distinguished from known hard polishing pads, which include micro porous polyurethane polishing pads that are relatively hard and not as compressible when compared to other types of polishing pads and polyurethane impregnated felt polishing pads. Examples of hard pads include the SUBA 1000 Series polishing pads and the SUBA® Pads available from Rodel in Phoenix, Ariz. -
FIG. 4 illustrates operation of theconditioning arm 110 according to an embodiment of the present invention. When thesoft polishing pad 108 is moving and awafer 106 is being polished, the conditioning arm 110 (and the diamond conditioner 112) remain in the position 402 situated adjacent to the perimeter of thesoft polishing pad 108. After a predetermined number of wafers have been polished by thesoft polishing pad 108, or when the polishing rate has been decreased due to build up of slurry and other debris, theconditioning arm 110 is pivoted at one end by thebase 107, lowered onto thesoft polishing pad 108, and swept along an arc indicated by the arrows 408 from the position 402 across the surface of the soft polishing pad 108 (as shown by phantom lines) to a second position 406 adjacent to the other side of the perimeter of the soft polishing pad 108 (also shown by phantom lines). -
FIG. 5 illustrates thediamond conditioner 112 according to an embodiment of the present invention. Thediamond conditioner 112 includes a base 502 havingdiamonds 504. The base 502 may be any suitable rigid substrate. Thediamonds 504 may be synthetic diamonds, natural diamonds, etc. - The
diamonds 504 may be placed on the base 502 using chemical vapor deposition (CVD). Alternatively, the diamonds 404 may be embedded in thebase 502. For example, thediamond conditioner 112 may be formed by embedding diamond particles in nickel coated on the surface of a rigid substrate according to well-known or proprietary techniques. - Embodiments of the invention can be implemented using hardware, software, firmware, or a combination of hardware and software. In implementations using software, the software may be stored on a computer program product (such as an optical disk, a magnetic disk, a floppy disk, etc.) or a program storage device (such as an optical disk drive, a magnetic disk drive, a floppy disk drive, etc.).
- The above description of illustrated embodiments of the invention is not intended to be exhaustive or to limit the invention to the precise forms disclosed. While specific embodiments of, and examples for, the invention are described herein for illustrative purposes, various equivalent modifications are possible within the scope of the invention, as those skilled in the relevant art will recognize. These modifications can be made to the invention in light of the above detailed description.
- In the above description, numerous specific details, such as particular processes, materials, devices, and so forth, are presented to provide a thorough understanding of embodiments of the invention. One skilled in the relevant art will recognize, however, that the embodiments of the present invention can be practiced without one or more of the specific details, or with other methods, components, etc. In other instances, well-known structures or operations are not shown or described in detail to avoid obscuring the understanding of this description.
- Various operations have been described as multiple discrete operations performed in turn in a manner that is most helpful in understanding embodiments of the invention. However, the order in which they are described should not be construed to imply that these operations are necessarily order dependent or that the operations be performed in the order in which the operations are presented.
- Reference throughout this specification to “one embodiment” or “an embodiment” means that a particular feature, structure, process, block, or characteristic described in connection with the embodiment is included in at least one embodiment of the present invention. Thus, the appearances of the phrases “in one embodiment” or “in an embodiment” in various places throughout this specification are not necessarily all referring to the same embodiment. Furthermore, the particular features, structures, or characteristics may be combined in any suitable manner in one or more embodiments.
- The terms used in the following claims should not be construed to limit the invention to the specific embodiments disclosed in the specification and the claims. Rather, the scope of embodiments of the invention is to be determined entirely by the following claims, which are to be construed in accordance with established doctrines of claim interpretation.
Claims (29)
1. A method of conditioning a chemical mechanical planarization (CMP) polishing pad, comprising:
conditioning a soft polishing pad using diamond conditioner by:
rotating the soft polishing pad on a platen;
rinsing the soft polishing pad; and
passing a diamond conditioner over the soft polishing pad.
2. The method of claim 1 , further comprising rinsing the soft polishing pad with deionized water.
3. The method of claim 2 , further comprising:
applying zero pounds per square inch (psi) to the soft polishing pad from the platen.
4. The method of claim 1 , wherein passing the conditioning arm having the diamond conditioner thereon over the soft polishing pad comprises passing the diamond conditioner over the soft polishing pad during wafer polishing.
5. The method of claim 1 , wherein passing the conditioning arm having the diamond conditioner thereon over the soft polishing pad comprises passing the diamond conditioner over the soft polishing pad between wafer polishings.
6. The method of claim 1 , further comprising rotating a wafer against the soft polishing pad.
7. The method of claim 6 , further comprising applying slurry to the surface of the soft polishing pad.
8. A chemical mechanical planarization (CMP) system, comprising:
a head mounted in a housing;
a wafer mounted to the head;
a platen mounted in the housing;
a soft polishing pad mounted to the platen;
a pad conditioning arm mounted in the housing; and
a diamond conditioner mounted to the pad conditioning arm.
9. The system of claim 8 , further comprising a slurry tank mounted in the housing.
10. The system of claim 9 , further comprising a water tank mounted in the housing.
11. The system of claim 8 , further comprising electromechanical equipment mounted in the housing.
12. The system of claim 8 , wherein the soft polishing pad comprises napped poromerics-porous urethane layers on a substantially compressible substrate.
13. (canceled)
14. The system of claim 8 , wherein the diamond conditioner comprises a diamond strip.
15. The system of claim 14 , wherein the diamond strip comprises synthetic diamonds embedded in a base.
16. The system of claim 8 , wherein the pad conditioning arm is to apply approximately 0.25 pounds per square inch (psi) to the soft polishing pad through the diamond conditioner.
17. The system of claim 8 , wherein the platen is to rotate during conditioning of the soft polishing pad.
18. The system of claim 17 , wherein the platen is to rotate at a rotational speed of approximately one hundred revolutions per minute (RPM).
19. The system of claim 18 , wherein the diamond conditioner is to make a single sweep across the soft polishing pad during conditioning of the soft polishing pad.
20. A chemical mechanical planarization (CMP) apparatus, comprising:
a soft polishing pad adhered to a platen in a housing, the soft polishing pad comprising a porous thermoplastic resin matrix reinforced with a felted mat of polyester fibers; and
a pad conditioning arm mounted in the housing, the pad conditioning arm having a diamond conditioner attached thereto, the diamond conditioner to condition the soft polishing pad.
21. The CMP apparatus of claim 20 , wherein the conditioning arm is to apply approximately 0.25 pounds per square inch (psi) to the soft polishing pad through the diamond conditioner.
22. The CMP apparatus of claim 20 , wherein the platen is to rotate during conditioning of the soft polishing pad.
23. The CMP apparatus of claim 22 , wherein the platen is to rotate at a rotational speed of approximately one hundred revolutions per minute (RPM).
24. The CMP apparatus of claim 20 , wherein the diamond conditioner is to make a single sweep across the soft polishing pad during conditioning of the soft polishing pad.
25. A chemical mechanical planarization (CMP) apparatus, comprising:
a housing having a platen;
a soft polishing pad adhered to the platen, the soft polishing pad comprising a felt sheet of fibers impregnated with micro porous elastomer; and
a pad conditioning arm mounted in the housing, the pad conditioning arm having a diamond conditioner attached thereto, the diamond conditioner to condition the soft polishing pad.
26. The CMP apparatus of claim 25 , wherein the platen is to rotate during conditioning of the soft polishing pad.
27. The CMP apparatus of claim 26 , wherein the soft polishing pad is to receive de-ionized (DI) water during conditioning of the soft polishing pad.
28. The CMP apparatus of claim 25 , wherein the diamond conditioner comprises diamond particles embedded in nickel coated on a surface of a rigid substrate.
29. The CMP apparatus of 28, wherein the diamond conditioner comprises synthetic and/or natural diamond particles.