DE2550487A1 - Correction layer for a correction material - comprises a pigment, binder, magnesium carbonate and aluminium silicate - Google Patents

Correction layer for a correction material - comprises a pigment, binder, magnesium carbonate and aluminium silicate

Info

Publication number
DE2550487A1
DE2550487A1 DE19752550487 DE2550487A DE2550487A1 DE 2550487 A1 DE2550487 A1 DE 2550487A1 DE 19752550487 DE19752550487 DE 19752550487 DE 2550487 A DE2550487 A DE 2550487A DE 2550487 A1 DE2550487 A1 DE 2550487A1
Authority
DE
Germany
Prior art keywords
correction
cover layer
binder
magnesium carbonate
correction material
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
DE19752550487
Other languages
German (de)
Inventor
Thadeusz Dudek
Bruno Dr Schmidt
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Kores Holding Zug AG
Original Assignee
Kores Holding Zug AG
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Priority to AT847975A priority Critical patent/AT354474B/en
Application filed by Kores Holding Zug AG filed Critical Kores Holding Zug AG
Priority to DE19752550487 priority patent/DE2550487A1/en
Priority to GB44022/76A priority patent/GB1514117A/en
Priority to BR7607301A priority patent/BR7607301A/en
Priority to FR7633474A priority patent/FR2330747A1/en
Priority to ES453033A priority patent/ES453033A1/en
Publication of DE2550487A1 publication Critical patent/DE2550487A1/en
Pending legal-status Critical Current

Abstract

A correction material comprises a support and a correction layer. The correction layer contains a pigment e.g. TiO2, is not >30 wt.% pref. 5-25 wt.% polystyrene, polyisoprene and/or polyterpene resin as binder, and additionally >10 pref. 15-80 most pref. 40-55 wt.% Mg carbonate and/or Al silicate. The correction layer is easily transferred by typing without any splitting or fracturing of this layer and accompanying fouling of the typewriter. The covering power of the material is excellent.

Description

KORREKTURMATERIALCORRECTION MATERIAL

Die vorliegende Erfindung betrifft ein Korrekturmaterial zum Abdecken von Zeichen, bestehend aus einem Träger und einer, auf diesem aufgebrachten Abdeckschicht, die aus einem Abdeckpigment, wie beispielsweise Titandioxyd und einem Bindemittel besteht.The present invention relates to a masking corrective material of signs, consisting of a carrier and a cover layer applied to it, that of a masking pigment, such as titanium dioxide and a binder consists.

Unter Zeichen können ganz allgemein falsch getippte Buchstaben oder Wörter verstanden werden0 Auch zum Ausbessern von Tuschzeichnungen oder gedruckten Markierungen eignet sich das erfindungsgemäße Komekturmaterial.In general, incorrectly typed letters or Understanding words0 Also for touching up ink drawings or printed ones The architectural material according to the invention is suitable for markings.

Das Unsichtbarmachen von falsch getippten Zeichen ist ein Problem, das so lange schon besteht, als mit der Schreibmaschine gearbeitet wird. Frither war man darauf beschränkt, Korrekturen durch Radieren oder Abkratzen vorzunehmen, wodurch zumeist das Trägerblatt beschädigt wurde und man unschöne Korrekturstellen erhielt.Making misspelled characters invisible is a problem that has existed as long as the typewriter is used. Frither one was limited to making corrections by erasing or scraping off, which mostly damaged the carrier sheet and left unsightly correction spots received.

In letzter Zeit entwickelte man eine Reihe von Korrekturmitteln, durch die das falsch getippte Zeichen abgedeckt wird.A number of corrective remedies have recently been developed which will cover the misspelled character.

Man hat versucht, stark deckende Weißpigmente in einem Lösungsmittel, entweder Wasser oder ein organisches Lösungsmittel, zu lösen oder zu dispergieren. Die Korrekturflüssigkeiten werden mittels eines Pinsels über das unsichtbar zu machende Zeichen aufgebracht. Der Nachteil derartiger Korrekturflüssigkeiten liegt insbesondere darin, daß sie kompliziert in der Handhabung sind, insbesondere sind es die langen Trocknungszeiten, die man auch bei den organische Lösungsmittel enthaltenden Korrekturflüssigkeiten nicht wesentlich verkürzen konnte, daß Korrekturflüssigkeiten nicht mit Erfolg angewendet werden konnten. Ein weiterer Nachteil liegt darin, daß das Papier an den überpinselten Stellen zur Wellenbildung neigt. Ein weiteres Problem ist das Ausbluten der Farbe des abzudeckenden Zeichens, wenn als Schreibbandfarbe organische Pigmente oder lösliche Farbstoffe verwendet werden, da das organische RFungsmittel das Pigment bzw.Attempts have been made to dissolve highly opaque white pigments in a solvent, either water or an organic solvent, to dissolve or disperse. The correction fluids are applied with a brush over the surface to be made invisible Sign applied. The disadvantage of such correction fluids is in particular in that they are complicated to use, especially the long ones Drying times are the same as for correction fluids containing organic solvents could not significantly reduce the fact that correction fluids were not used successfully could become. Another disadvantage is that the paper is brushed over Tends to form waves. Another problem is bleeding of the paint of the character to be covered if the writing tape color is organic or soluble pigments Dyes are used because the organic agent removes the pigment or

den Farbstoff anlöst.dissolves the dye.

Verwendet man Dispersionen auf wässriger Basis, so setzt sich nach relativ kurzer Zeit das Kunstharz am Boden des Aufbewahrungsgefäßes ab, da. die Dispersionen nicht stabil sind, was durch die Koagulierung des Kunstharzes bedingt ist. Die Folge ist, daß die Korrekturflüssigkeiten nach relativ kurzer Zeit unbrauchbar sind.If water-based dispersions are used, it will settle relatively short time, the synthetic resin at the bottom of the storage vessel, because. the Dispersions are not stable, which is due to the coagulation of the synthetic resin is. The consequence is that the correction fluids become unusable after a relatively short time are.

Nicht umsonst haben am meisten die sogenannten Korrekturblättchen im Bürobetrieb Anklang gefunden. Sie bestehen aus einem Trägermaterial, auf das eine Abdeckschicht mit einem hohen Anteil von Abdeckpigmenten, eingebettet in ein Bindemittel, aufgebracht ist. Als Abdeckpigment kommt hauptsächlich Titandioxyd in Betracht. Titandioxyd ist zwar ein sehr stark deckendes Pigment, bringt aber den Nachteil mit sich, daß die mittels Titandioxyd als Hauptkomponente enthaltenden Korrekturblättohen abgedeckten Zeichen schlecht überschreibbar sind. Der hohe Gehalt an Titandioxyd ist zumeist auch die Ursache, daß die Korrekturblättchen stark abfärben bzw. deren Abdeckschicht zum Absplittern neigt, was eine starke Verschmutzung der Schreibmaschine zur Folge hat. Als Bindemittel wurden hauptsächlich wachsartige Stoffe verwendet, wie Hartcerisine, gereinigte Montanharze oder synthetische Wachse, Chlornaphthaline, Polyäthylene, Polyvinylchlorid, Polyvinylazetat, Polystyrol, Äthylzellulose und viele andere. Auch durch einen Zusatz von sogenannten Haftmitteln, als die Natur- und Kunstharze, z. B. Kolophonium oder Weichharze, wie Polyvinylharze, Polyisobutylen oder Aluminiumsalze eines Additionsproduktes aus Phenolresol mit Abietinsäure in Betracht kamen, konnte man keine zufriedenstellenden Ergebnisse erzielen.It is not for nothing that most of them have the so-called correction sheets met with approval in office operations. They consist of a carrier material on which a cover layer with a high proportion of cover pigments, embedded in a Binder, is applied. The main masking pigment used is titanium dioxide into consideration. Titanium dioxide is a very good covering pigment, but it does with the disadvantage that the means containing titanium dioxide as the main component Characters covered by correction sheets are difficult to overwrite. The high salary Titanium dioxide is usually the reason why the correction sheets stain heavily or their cover layer tends to splinter, which leads to severe contamination of the Typewriter. The main binders used were waxy Substances used, such as hard ceria, purified montane resins or synthetic waxes, Chloronaphthalenes, polyethylene, polyvinyl chloride, polyvinyl acetate, polystyrene, ethyl cellulose and many others. Also through the addition of so-called adhesives, as the natural and synthetic resins, e.g. B. rosin or soft resins such as polyvinyl resins, polyisobutylene or aluminum salts of an addition product of phenol resol with abietic acid in However, satisfactory results could not be obtained.

Der Begriff Haftmittel bzw. Bindemittel ist nicht genau definiert, es läßt sich nicht angeben, ob ein Zusatz als Bindemittel oder Haftmittel anzusprechen ist. Es wird beiden praktisch die gleiche Funktion zugeschrieben, nämlich die Haftung des Pigmentes an der Trägerfolie zu gewährleisten bzw. ein konturentreues Ubertragen auf das zu überdeckende Zeichen zu bewirken.The term adhesive or binding agent is not precisely defined, it cannot be stated whether an additive should be addressed as a binder or an adhesive is. Practically the same function is ascribed to both, namely liability of the pigment on the carrier film or a true-to-contour transfer to cause the character to be covered.

Man konnte bis jetzt noch keine zufriedenstellenden Ergebnisse erzielen, da durch die herkömmlich Zusammensetzung zumindest einer der Nachteile in Kauf genommen werden muß, daß entweder das zu korrigierende Zeichen unzureichend überdeckt wird, so daß die Schrift wieder sichtbar wird oder die Korrekturschicht zu stark abblättert und die Schreibmaschine verschmutzt oder die korrigierte Stelle schlecht zu übertippen ist. Bei Farbbändern mit organischen Farbstoffen kommt noch hinzu, daß die korrigierten Stellen zum Ausbluten neugen. Kugelschreiberschrift konnte bis jetzt kaum dauerhaft überdeckt werden.Satisfactory results have not yet been achieved because at least one of the disadvantages is accepted due to the conventional composition must be that either the character to be corrected is insufficiently covered, so that the writing becomes visible again or the correction layer flakes off too much and the typewriter is dirty or the corrected part is badly typed over is. In the case of ribbons with organic dyes, there is also the fact that the corrected ones Prone to bleeding. Until now, ballpoint pen could hardly be permanent are covered.

Man hat eine Reihe von Verbesserungsvorschlägen gemacht, mußte jedoch immer wieder feststellen, daß die Verbesserung der einen Eigenschaft eine qualitative Verschlechterung der anderen Eigenschaft zur Folge hatte. Ein weiteres Problem bei Korrekturmitteln der erfindungsgemäßen Art ist darin zu sehen, daß die Abdeckschicht auf dem Trägermaterial zwar gut haften muß, die Affinität zum Schreibpapier, auf dem die Korrekturen angebracht werden sollen, Jedoch so groß ist, daß die konturengetreue Übertragung der Abdeckmasse auf das falsch getippte Zeichen gewährleistet ist.A number of suggestions for improvement were made, but had to be keep finding that the improvement of one property is a qualitative one Worsening of the other property. Another problem with Correction means of the type according to the invention can be seen in the fact that the cover layer the affinity to the writing paper must adhere well to the carrier material to which the corrections are to be made, However, it is so large that the contour is true to the contour Transfer of the masking compound to the incorrectly typed character is guaranteed.

Dieses Problem hat man versucht, durch einen Zusatz von Aluminium in Plättchenform zu der Beschichtungsmasse der Korrektrblätter zu lösen.Attempts have been made to solve this problem by adding aluminum in platelet form to solve the coating mass of the correct sheets.

Das Durchbluten der überdeckten Farbe hat man versucht dadurch auszuschalten, daß man der Abdeckschicht Adsorptionsmittel wie Ton oder Talk zugesetzt hat, um eine dichtere und saubere Abdeckung zu erzielen.The bleeding of the covered color was tried to be switched off by that one has added adsorbents such as clay or talc to the cover layer to achieve a denser and cleaner coverage.

Durch Variation der Lösungsmittel wollte man ebenfalls die Ergebnisse verbessern. Ein Vorschlag geht dahin, ein Lösungsmittel auszuwählen, das das Bindemittel nicht löst, sondern lediglich leicht anquillt. Dadurch gedachte man, eine Auflockerung der Schichtstruktur zu erreichen, was die Übertragung des Korrekturmaterials auf die zu korrigierende Unterlage verbessern sollte.By varying the solvents one wanted the results as well to enhance. One suggestion is to select a solvent that will be the binder does not dissolve, but just swells slightly. This was thought to be a loosening up the layer structure to achieve what the transfer of the correction material on the document to be corrected should improve.

Es war auch nicht möglich, durch Aufbringen einer Haftvermittlungsschicht über der Pigmentschicht zufriedenstellende Ergebnisse bei der konturgetreuen Übertragung der Abdeckschicht zu erzielen.It was also not possible by applying an adhesion-promoting layer Satisfactory results in true-to-contour transfer over the pigment layer to achieve the cover layer.

Bisher war es so, daß man stets nur eines der Probleme zufriedenstellend lösen konnte, man erhielt entweder ein Korrekturmaterial, das zufriedenstellende Abdeckeigenschaften ohne Neigung zum Abblättern bzw. Absplittern der Abdeckschicht zeigte, jedoch war die Übertippbarkeit der korrigierten Zeichen völlig unzureichend, oder man konnte zwar die Ubertippbarkeit verbessern, was durch einen Zusatz von Magnesiumsilikaten möglich ist, erhielt jedoch stark abblätternde bzw. absplitternde Abdeckschichten.So far it has always been the case that only one of the problems is satisfactory could solve, you either got a corrective material that was satisfactory Covering properties without a tendency to flake or splinter the cover layer showed, but the typability of the corrected characters was completely inadequate, or the typability could be improved, which could be achieved by adding Magnesium silicates is possible, but got heavily flaking or chipping off Covering layers.

Durch die vorliegende Erfindung konnte ein Korrekturmaterial der eingangs erwähnten Art geschaffen werden, dessen Abdeckmasse gut übertippbare Korrekturstellen ergibt. Das Abblättern bzw. Absplittern der Schicht konnte praktisch zur Gänze beseitigt werden, so daß sich keine Verschmutzungen der Schreibmaschine mehr ergeben.Through the present invention, a correction material could be the initially mentioned type are created, the covering compound can be easily typed over correction points results. The peeling or chipping of the layer could practically be completely eliminated so that the typewriter is no longer dirty.

Auch die Abdeckeigenschaften der erfindungsgemäßen Korrekturmaterialien sind weit verbessert worden.Also the covering properties of the correction materials according to the invention have been vastly improved.

Die Erfindung besteht darin, daß die Abdeckschicht neben dem üblichen Abdeckpigment, wie Titandioxyd, zusätzlich Magnesiumsilikat und/oder Aluminiumsilikat und als Bindemittel Copolymere von Polystyrol und Polyisopren und/oder Polyterpenharze enthält.The invention consists in that the cover layer in addition to the usual Covering pigment, such as titanium dioxide, plus magnesium silicate and / or aluminum silicate and copolymers of polystyrene and polyisoprene and / or polyterpene resins as binders contains.

Ausgezeichnete Resultate erzielt man, wenn das Magnesiumkarbonat und/oder Aluminiumsilikat in einer Menge von mindestens 10 Ges.% vorhanden ist.Excellent results are achieved when the magnesium carbonate and / or Aluminum silicate is present in an amount of at least 10% by weight.

Das Bindemittel kann in einer Menge bis zu 30 Ges.%, vorzugsweise 5 - 25 Gew.% der Abdeckschicht einverleibt sein.The binder can be used in an amount of up to 30% by weight, preferably 5 - 25% by weight of the cover layer can be incorporated.

Wird der Abdeckschicht lediglich Magnesiumkarbonat und/oder Aluminiumsilikat einverleibt, kann man zwar die Übertippbarkeit verbessern, jedoch neigt das Korrekturmaterial zum Abblättern bzw. Absplittern. Erst durch die gezielte Auswahl des Bindemittels konnte man auch das nachteilige Abblättern bzw. Absplittern der Abdeckschicht beseitigen.If the cover layer is only magnesium carbonate and / or aluminum silicate incorporated, the over-typability can be improved, but the correction material tends to be for flaking or chipping. Only through the targeted selection of the binding agent you could also see the disadvantageous flaking or chipping of the Cover layer remove.

Das Magnesiumkarbonat und/oder Aluminiumsilikat kann in einer Menge von 15 - 80 Gew.%, vorzugsweise 40 - 55 Gew.% in der Abdeckschicht vorhanden sein.The magnesium carbonate and / or aluminum silicate can be used in an amount of 15-80% by weight, preferably 40-55% by weight, may be present in the cover layer.

Der Abdeckschicht können zusätzlich Dispergiermittel, wie beispielsweise alkylmodifizierte Polyvinylpyrrolidonverbindungen zugesetzt sein.The cover layer can also contain dispersants, such as, for example alkyl-modified polyvinylpyrrolidone compounds may be added.

Es versteht sich von selbst, daß man je nach Bedarf weitere Zusätze der Abdeckschicht beimischen kann, wie beispielsweise übliche Netzmittel, Homogenisiermittel und dergleichen.It goes without saying that further additives can be used as required can be admixed with the cover layer, such as, for example, customary wetting agents, homogenizing agents and the same.

Ein weiterer Vorteil der Erfindung ist darin zu erblicken, daß man bei der Auswahl*-des Trägermaterials nicht nur auf stark saugende Folien, wie Papier beschränkt ist, sondern auch Kunststoffolien auf Basis von Polyäthylen oder Polypropylen und sogar Metallfolien verwenden kann.Another advantage of the invention is to be seen in the fact that one When choosing * the carrier material, do not only use highly absorbent foils such as paper is limited, but also plastic films based on polyethylene or polypropylene and can even use metal foils.

Die vorliegende Erfindung eignet sich nicht nur für Korrekturmatadal in Blättchenform, sondern kann auch auf einen Träger in Bandform aufgebracht werden, der als Korrekturband in der Schreibmaschine läuft. Gute Ergebnisse lassen sich mit der vorliegenden Erfindung auch erzielen, wenn man ein zur Hälfte eingefärbtes Farbband an seiner zweiten Hälfte mit der erfindungsgemäßen Abdeckschicht versieht.The present invention is not only suitable for correction matadal in sheet form, but can also be applied to a carrier in tape form, which runs as a correction tape in the typewriter. Good results can be achieved also achieve with the present invention if you have a half-colored Provides ribbon on its second half with the cover layer according to the invention.

Die Erfindung soll nun anhand einiger AusfUhrungsbeispiele näher erläutert werden.The invention will now be explained in more detail with the aid of a few exemplary embodiments will.

Beispiel 1: Auf einem Papierträger wurde eine Beschichtungsmasse folgender Zusammensetzung aufgebracht: Titandioxyd 12 Gew.T.Example 1: A coating composition was made as follows on a paper support Composition applied: Titanium dioxide 12 parts by weight

Aluminiumsilikat 15 " Copolymere von Polystyrol und Polyisopren 1,5 " Die Beschichtungsmasse wurde in einer Menge von 14 g pro m2 aufgebracht.Aluminum silicate 15 "copolymers of polystyrene and polyisoprene 1.5 "The coating compound was applied in an amount of 14 g per m2.

Beispiel 2: Auf eine Trägerfolie aus Polypropylen wurde folgende Beschichtungsmasse aufgebracht: Titandioxyd 15 Gew.T.Example 2: The following coating material was applied to a polypropylene carrier film applied: titanium dioxide 15 parts by weight.

Magnesiumkarbonat 3 1I Aluminiumsilikat 11 " Polyterpenharze 5 II Dispergiermittel (Polyvinylpyrrolidon) 0,2 " Die Abdeckmasse wurde in einer Menge von 15 g pro m2 Trockengewicht auf den Träger aufgebracht.Magnesium carbonate 3 1I aluminum silicate 11 "polyterpene resins 5 II Dispersant (polyvinylpyrrolidone) 0.2 "The masking compound was in an amount of 15 g per m2 dry weight applied to the carrier.

Beispiel 3: Auf eine Aluminiumfolie wurde folgende Abdeckmasse aufgebracht: Titandioxyd 10 Gew.T.Example 3: The following cover compound was applied to an aluminum foil: Titanium dioxide 10 parts by weight

Aluminiumsilikat 1 " Magnesiumkarbonat 7 lt Copolymere von Polystyrol und Polyisopren 3 n Polyterpenharze 1,5 lt Dispergiermittel (modifiziertes Polyvinylpyrrolidon) 0,1 n Die Auftragsstärke betrug 12 g pro m2 Trockengewicht.Aluminum silicate 1 "Magnesium carbonate 7 lt copolymers of polystyrene and polyisoprene 3 n polyterpene resins 1.5 lt dispersant (modified polyvinylpyrrolidone) 0.1 n The application thickness was 12 g per m2 dry weight.

Es versteht sich von selbst, daß man im Rahmen der vorliegenden Erfindung die Komponenten der Abdeckschicht beliebig miteinander kombienieren kann. Man wird auf alle Fälle Qualitä.tsverbesserungen gegenüber den bisher bekannten Korrekturmaterialien erzielen.It goes without saying that within the scope of the present invention the components of the cover layer can be combined with one another as desired. You will In any case, quality improvements compared to the previously known correction materials achieve.

Claims (6)

P A T E N T A N S P R Ü c H E 1) Korrekturmaterial zum Abdecken von Zeichen, bestehend aus einem einem Träger und einer auf diesem aufgebrachten Abdeckschicht, die ein Abdeckpigment, wie Titandioxyd, und ein Bindemittel enthält, dadurch gekennzeichnet, daß die Abdeckschicht zusätzlich Magnesiumkarbonat undZoder Aluminiumsilikat und als Bindemittel Copolymere von Polystyrol und Polyisopren und/oder Polyterpenharze enthält. P A T E N T A N S P R Ü c H E 1) Correction material to cover Sign, consisting of a carrier and a cover layer applied to it, which contains a covering pigment, such as titanium dioxide, and a binder, characterized in that that the cover layer additionally magnesium carbonate and Z or aluminum silicate and as binders, copolymers of polystyrene and polyisoprene and / or polyterpene resins contains. 2) Korrekturmaterial nach Anspruch 1, dadurch gekennzeichnet, daß die Abdeckschicht mindestens 10 Gew.% Magnesiumkarbonat und/oder Aluminiumsilikat enthält. 2) correction material according to claim 1, characterized in that the cover layer at least 10% by weight magnesium carbonate and / or aluminum silicate contains. 3) Korrekturmaterial nach Anspruch 1 oder 2, dadurch gekennzeichnet, daß die Abdeckschicht Magnesiumkarbonat und/oder Aluminiumsilikat in einer Menge von 15 bis 80 Gew.%, vorzugsweise 40 bis 55 Gew.% enthält. 3) correction material according to claim 1 or 2, characterized in that that the cover layer is magnesium carbonate and / or aluminum silicate in an amount Contains from 15 to 80% by weight, preferably from 40 to 55% by weight. 4) Korrekturmaterial nach einem oder mehreren der Ansprüche 1 bis 3, dadurch gekennzeichnet, daß die Abdeckschicht bis zu 30 Gew.% Copolymere von Polystyrol und Polyisopren und/oder Polyterpenharze enthält. 4) Correction material according to one or more of claims 1 to 3, characterized in that the cover layer up to 30 wt.% Copolymers of Contains polystyrene and polyisoprene and / or polyterpene resins. 5) Korrekturmaterial nach einem oder mehreren der Ansprüche 1 bis 4, dadurch gekennzeichnet, daß die Abdeckschicht als Bindemittel 5 bis 25 Gew.% Copolymere von Polystyrol und Polyisopren und/oder Polyterpenharze enthält. 5) Correction material according to one or more of claims 1 to 4, characterized in that the cover layer is used as a binder 5 to 25 wt.% Contains copolymers of polystyrene and polyisoprene and / or polyterpene resins. 6) Korrekturmaterial nach einem oder mehreren der Ansprüche 1 bis 5, dadurch gekennzeichnet, daß die Abdeckschicht zusätzlich Dispergiermittel, beispielsweise alkylmodifizierte Polyvinylpyrrolidonverbindungen, Homogenisiermittel und Netzmittel enthält. 6) Correction material according to one or more of claims 1 to 5, characterized in that the cover layer additionally dispersants, for example alkyl modified polyvinylpyrrolidone compounds, homogenizing agents and wetting agents contains.
DE19752550487 1975-11-07 1975-11-11 Correction layer for a correction material - comprises a pigment, binder, magnesium carbonate and aluminium silicate Pending DE2550487A1 (en)