CA1133009A - Process for the preparation of urethane - Google Patents

Process for the preparation of urethane

Info

Publication number
CA1133009A
CA1133009A CA345,675A CA345675A CA1133009A CA 1133009 A CA1133009 A CA 1133009A CA 345675 A CA345675 A CA 345675A CA 1133009 A CA1133009 A CA 1133009A
Authority
CA
Canada
Prior art keywords
nitro
compounds
reaction
compound
elements
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
CA345,675A
Other languages
French (fr)
Inventor
Robert Becker
Johann Grolig
Christian Rasp
Gunter Stammann
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Bayer AG
Original Assignee
Bayer AG
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Bayer AG filed Critical Bayer AG
Application granted granted Critical
Publication of CA1133009A publication Critical patent/CA1133009A/en
Expired legal-status Critical Current

Abstract

Mo-2034 LeA 19,484 PROCESS FOR THE PREPARATION OF URETHANE
ABSTRACT OF THE DISCLOSURE
Production of urethanes by the oxycarbonylation reaction of N,N'-disubstituted ureas and organic com-pounds containing at least one hydroxyl group with carbon monoxide in the presence of molecular oxygen and/or organic nitro compounds and a catalyst system comprising (a) a noble metal and/or noble metal compound of the eighth subgroup of the periodic system of elements and (b) a compound of an element and/or elements of the third to fifth main group and/or first to eighth sub-group of the periodic system of elements characterized in that said compounds are capable of undergoing Redox reactions under the reaction conditions.

LeA 19,484

Description

11~

-1- Mo-2034 LeA 19,484 PROCESS FOR THE PREPARATIO~ OF URETHANE
~IELD O~ TH~ INVENTION
This invention relates to an improved process or the preparation of urethane from N, N ' -disubstituted ureas and organic compounds containing at least one hydroxyl group.
BACKGROUND OF THE INVENTION
Organic isocyanates are generally produced on a large commercial scale by the reaction of the corres-ponding amines with phosgene. Because of the toxicityof phosgene, considerable time has been spent trying to find a method of synthesis of organic isocyanates which would eliminate the need for phosgene. One such method consists of reacting organic nitro compounds with carbon monoxide and organic hydroxyl compounds to the corresponding urethanes and then decomposing these into isocyanates and compounds containing hydroxyl groups.
This decomposition reaction can be preceded by a modification of the urethane obtained as intermediate product. Thus, for example, the urethane obtainable from nitrobenzene, carbon monoxide and ethanol could first be reacted with formaldehyde to form the bis-urethane of 4,4'-diisocyanatodiphenyl methane, which could then be converted into 4,4'-diisocyanatodiphenyl methane with elimination of the ethanol.
The decomposition of urethanes into the corres-ponding isocyanates and hydroxyl compounds has been described, for example, in German Offenlegungsschrift
2,421,503 and the prior publication cited therei~.
Methods for the preparation of urethanes described in th~ patent literature include the reaction of nitro compounds with carbon monoxide and alcohols in the presence of selenium or selenium compounds (German Offen-legungsschriften 2,343,826 (U.S. 3,895,054): 2,614,101 and LeA 19,484 ~.~

11~3~09 2,623,694 (U.S. 4,080,365) or of noble metals, in particular palladium, in the presence of Lewis acids (German Offenlegungsschriften 1,568,044 and 2,603,574).
For the preparation of a mononitro compound, this reaction proceeds in accordance with the following stoichiometric equation:
R - NO2 + 3CO + R'OH ~ RNHCO2R' + 2CO2.
The general reaction equation is as follows:
R(NO2)X + 3xCO + xR'OH + R(NHCO2R')X + 2xCO2.
This means that for each mol of urethane group to be produced three mols of carbon monoxide are used up and two mols of carbon dioxide are formed. Only one-third of the carbon monoxide put into the process is used for the formation of urethane groups. Two-thirds are converted into the technically useless inert carbon dioxide. Large amounts of heat are evolved in the exothermic formation of carbon dioxide.
Therefore, expensive equipment for removing the heat of reaction is necessary in the known industrial method of synthesizing a urethane from a nitro compound, carbon monoxide and alcohol.
The patent literature also teaches how to react N,N'-dialkyl ureas or N,N'-diaryl ureas with alcohols to produce a urethane and an amine, for example, U. S.
Patent 2,409,712. The following represents this reaction scheme:
RNHCONHR + R'OH ) RNHCO2R' + RNH2.
In this method, however, only one-half of the alkyl or aryl groups in the urea is converted into urethane while the other half is converted to the free amine.

LeA 19,484 - ~330,0, 9 DESCRIPTION OF THE INVENTION
It has now been found that N,N'-disubstituted ureas can be reacted with organic compounds containing at least one hydroxyl group to produce urethanes without free amine being split off in the process. The yield, based on N,N'-disubstituted urea, is therefore virtually doubled. This is accomplished where ureas together with organic compounds containing at least one hydroxyl group are subject to an oxycarbonylation with carbon monoxide under specific reaction conditions.
The present invention thus relates to a process for the preparation of urethanes comprising reacting N,N'-disubstituted ureas and organic compounds having at least one hydro~yl group, characterized in that these starting compounds are subjected to an oxycarbonyl-ation in the presence of carbon monoxide and molecular oxygen and/or organic nitro compounds as oxidizing agent and a catalyst comprising:
(a) . a noble metal and/or a noble metal compound of the eighth sub-group of the periodic system of elements-and (b) a compound of elements of the third to fifth main group and/or first to eighth subgr~u~ of the periodic system of elements, other than the compounds Of group (a) which compound is capable of undergoing Redox reactions un~er the reaction conditions.
The N,N'-disubstituted ureas suitable as starting materials for the instant process may be any ureas of this type which are substituted with an organic group.
~hey may also contain nitro groups in which case the addition ~f other nitro compounds may be omitted. They generally have a molecular weight of from 88 to 500, preferably from 212 to 330. The starting materials LeA 19,484 ~33009 also include any organic compounds containing at least one hydroxyl group, for example, substituted aliphatic, cycloaliphatic and/or aromatic monohydroxyl or poly-hydroxyl compounds. These compounds generally have a molecular weight in the range of from 32 to 300, preferably from 32 to 102.
The organic substituents on the N,N'-disubstituted ureas may be the same or different. They may be aliphatic, cycloaliphatic or aromatic groups. Examples of these groups are methyl; ethyl; ethylene; propyl;
isopropyl; 1,2-propylene; 1,3-propylene; butyl; isobutyl;
sec.-butyl and tert.-butyl groups.
Further examples of suitable groups are the pentyl;
hexyl; heptyl; octyl; decyl; dodecyl; cetyl; cyclopentyl;
cyclohexyl; phenyl; p-tolyl; o-tolyl; m-tolyl; o-chloro-phenyl; p-chlorophenyl; m-chlorophenyl; o-aminophenyl;
p-aminophenyl; m-aminophenyl; o-nitrophenyl; p-nitro- .
phenyl and m-nitrophenyl groups. 3-amino-2-methyl phenyl;
3-amino-4-methyl phenyl; 5-amino-2-methyl phenyl; 3-nitro-2-methyl phenyl; 3-nitro-4-methyl phenyl; 5-nitro-2-methyl phenyl; l-naphthyl; 2-naphthyl; 6-amino-1-naphthyl and 6-nitro-1-naphthyl are also suitable groups.
N,N'-disubstituted ureas containing aromatic groups are preferred. Examples of these preferred ureas are N,N'-diaryl ureas. Specific suitable examples are N,N'-diphenyl urea, N,N'-di-(p-tolyl)-urea; N,N'-di-(o-tolyl)-urea; N,N' di-(o-aminophenyl)-urea; N,N'-di-(p-aminophenyl)-urea;
N,N'-di-(o-nitrophenyl)-urea; N,N'-di-(3-amino-2-methyl phenyl)-urea; N,N'-di-(3-amino-4-methyl phenyl)-urea;
N,N'-di-(5-amino-2-methyl phenyl)-urea; N,N'-di-(3-nitro-
4-methyl phenyl)-urea; N,N'-di-(5-nitro-2-methyl phenyl)-urea and N,N'-di-(3-nitro-2-methyl phenyl)-urea.

LeA 19,484 ~3009 N-(3-amino-2-methyl phenyl)-N'-(3-nitro-2-methyl phenyl)-urea; N-(3-amino-4-methyl phenyl)-N'-(3-nitro-4-metllyl phenyl)-urea; N-(5-amino-2-methyl phenyl)-N'-(5-nitro-2-methyl phenyl)-urea; N-(3-amino-2-methyl phenyl)-N'-(5-amino-2-methyl phenyl)-urea; N-(3-amino-2-methyl phenyl)-N'-(3-amino-4-methyl phenyl)-ureai ~-(3-amino-4-methyl phenyl)-N'-(5-amino-2-methyl phenyl)-urea;
N-(3-nitro-2-methyl phenyl)-N'-(5-amino-2-methyl phenyl)-urea; N-(3-nitro-2-methyl phenyl)-N'-(5-nitro-2-methyl phenyl)-urea are also examples of specifically suitable N,N'-diaryl ureas. The following are particularly preferred: N,N'-diphenyl urea; N,N'-di-(p-tolyl)-urea;
N,N'-di-(o-tolyl)-urea; N,N'-di-(3-amino-2-methyl phenyl)-urea; N,N'-di-(3-amino-4-methyl phenyl)-urea;
and N,N'-di-(5-amino-2-methyl phenyl)-urea. Also preferred are the corresponding asymmetric N,N'-di-substituted diaryl ureas which are amino or methyl substituted on the aromatic rings, and any mixtures of these compounds.
The starting materials for the instant process also includes any organic compounds containing hydroxyl groups. Examples are any monohydric or polyhydric alcohols or monovalent or polyvalent phenols. Suitable alcohols include, for example, those having a molecular weight in the range of 32 to 300. These may include linear or branched chain monohydric or polyhydric alkanols or alkenols as well as any monohydric or polyhydric cycloalkanols, cycloalkenols or aralkyl alcohols.
The alcohols may also carry any inert substituents such as, for example, halogen atoms, sulphoxide groups, sulphone groups, carbonyl groups or carboxylic acid ester groups. Alcohols having ether bridges are also LeA 19,484 ~1133~)09 suitable in principle. The following are examples of suitable alcohols: methanol, ethanol~ n-propanol, isopropa~ol, n-butanol, n-pentanol, n-hexanol, cyclo-hexanol, benzyl alcohol, chloroethanol, ethylene glycol, diethylene glycol, propyiene glycol, dipropylene glycol, glycerol, hexane-triol and trimethylol propane.
Monohydric aliphatic alcohols having l to 6 carbon atoms are preferably used.
Suitable phenols include, in particular, those within a molecular weight range of 94 to 300. Examples are phenol, the isomeric chlorophenols, cresols, ethyl phenols, propyl phenols, butyl phenols or higher alkyl phenols. Pyrocatechol, 4,4'-dihydroxy-diphenyl methane, bisphenol-A, anthranol, penanthranol, pyrogallol or phloroglucinol are also suitable. The alcohols exemplified above are preferred over the exemplified phenols. Ethanol is the particularly preferred hydroxyl compound to be used in the instant process.
The organic hydroxyl compounds are generally used in such quantities, in the instant process, that the reaction mixture contains from l to lOO hydroxyl groups for each urethane group to be formed. When calculating the quantity of hydroxyl compound required, it should be taken into account that when amino substituted ureas are used or when nitro compounds are present in the reaction mixture, the amino and nitro groups are also converted into urethane groups.
That is, one equivalent of hydroxyl groups is required for each mol of urea as well as for each mol of amino or nitro groups in the stoichiometric reaction.
Carbon monoxide is used as the other reactant in the instant process. This starting material is generally used in a quantity corresponding to l to 30 LeA 19,484 ~33009 mol per mol of urethane to be produced. ~hen calculating this quantity, the fact that, in the stoichiometric reaction, l mol of carbon monoxide is required for each mol of urea and each mol of amino or nitro groups present in the reaction mixture must be taken into account.
The reaction according to the instant invention is carried out in the presence of oxidizing agents and catalysts.
The oxidizing agent used may be molecular oxygen in the pure form or in the form of mixtures with inert gases such as nitrogen or carbon dioxide, in particular in the form of air. In the presence of molecular oxygen, oxycarbonylation proceeds in accordance with the following reaction equation:
R1NHCONHR2 + ~2 + CO + 2R'OH
R NHCO2R' + R2NHCO2R' = H2O
wherein Rl may be different from R2, but Rl and R2 are preferably the same.
Organic nitro compounds are the preferred oxidizing agents. Any of a wide variety of nitro compounds may be used. Under the conditions of oxycarbonylation, these are also converted into urethanes, for example, according to the followlng reaction equation:
2RlNHCONHR2 f R NO2 + 3CO + 5R'OH
2RlNHC02R' + 2R2NHC02R' f R3NHCo2R' + 2H20 It is particularly preferred to carry out the reaction of symmetric N,N'-diaryl ureas in the presence of an aromatic nitro compound in which the aryl group is the same as the aryl groups of the urea. Oxycar-bonylation then proceeds in accordance with the LeA 19,484 following equation to form a single urethane:
2~1HCONHR + RNO2 + 3CO + 5R'OH >
5RNHCO2R' + 2~2 To realize optimum yield when using organic nitro compounds as the sole oxidizing agents, the quantities of urea compound and nitro compound are preferably calculated to provide two mols of urea for each mol of nitro groups in the reaction mixture.
When amine substituted ureas are used, however, it must be remembered that an additional half mol of nitro groups is necessary for each mol of amino groups in order to convert the amino groups into urethane groups.
When nitro substituted ureas are used, it is of course necessary to provide an additional oxidizing agent, provided the quantity of nitro groups present is sufficient for the stoichiometric conversion to urethane.
To realize optimum yields when molecular oxygen is used as the sole oxidizing agent in the above reaction e~uation, at least one half mol of oxygen must be present for each mol of urea. If amino groups are present, at least one half mol of oxygen must also be available for each mol of amino groups. The oxygen may be used in excess Le~s than e~uivalent quantities of oxygen would reduce the yield. It is advantageous to add an inert gas such as nitrogen or carbon dioxide in such quantities that the reaction can be carried out without the risk of explosion of the mixtures of oxygen and carbon monoxid or mixtures of oxygen and alcohol. If no inert gas is added, the quantity of oxygen used should be calculated to avoid the formation of explosive mixtures with carbon monoxide and the alcohol component. Molecular oxygen is preferably LeA l9 r 484 ,, li~9 _9_ used in the form of air or of mixtures of air and nitrogen.
Oxygen and a nitro compound may be used together as oxidizing agents in which case the ni~ro compound may be used in less than the stoichiometric quantity.
The oxidizing agents may be added in excess so that when nitro compounds are used they may be added in quantities providing a molar ratio of urea to nitro groups ranging from 1:1 to 4:1, in particular from l.S:l to 2.5:1 and most preferably from 1.8:1 to 2.2:1.
The nitro compounds used for the instant process may be any organic compounds, generally with molecular weights from 61 to 400, preferably from 123 to 262, having at least one aliphatically, cycloaliphatically and/or aromatically bound nitro group.
The following are examples of suitable aromatic nitro compounds: nitrobenzene; o-dinitrobenzene; m-dinitrobenzene; p-dinitrobenzene; o-chloro nitrobenzene;
m-chloro-nitrobenzene; o-chloro-nitrobenzene; o-nitro-toluene; m-nitrotoluene and p-nitrotoluene. Also suitable are o-amino-nitrobenzene; m-amino-nitrobenzene;
p-amino-nitrobenæene; 2-amino-3-nitrotoluene; 3-amino-2-nitrotoluene; 2-amino-4-nitrotoluene; 4-amino-2-nitrotoluene; 2-amino-5-nitrotoluene; 2-amino-6-nitrotoluene; 5-amino-2-nitrotoluene; 3-amino-4-nitrotoluene; 4-amino-3-nitrotoluene; 3-amino-4-nitrotoluene and 3-amino-5-nitrotoluene. 2,3-dinitro-toluene; 2,4-dinitrotoluene; 2,5-dinitrotoluene; 2,6-dinitrotoluene; 3,4-dinitrotoluene; 3-nitro-o-xylene;
4-nitro-o-xylene; 2-nitro-m-xylene; 5-nitro-m-xylene;
nitro-p-xylene; 3,4-dinitro-o-xylene; 3,5-dinitro-o-xylene; 3,6-dinitro-o-xylene; 4,5-dinitro-o-xylene;

~eA 19,484 ~330~

2,4-dinitro-m-xylene; 2,5-dinitro-m-xylene; 4,5-dinitro-m-xylene; 4,6-dinitro-m-xylene; 2,3-dinitro-p-xylene;
2,6-dinitro-p-xylene are also suitable compounds.
Still more examples of suitable compounds are l-nitro-naphthalene; 2-nitronaphthalene; dinitronaphthalenes;
nitroanthracenes; nitro-diphenyls; bis-(nitrophenyl)-methanes; bis-(nitrophenyl)-thio-ethers; bis-(nitro-phenyl)-sulphones; nitrodiphenoxy alkanes and nitro-phenothiazines.
The following are suitable cycloaliphatic nitro compounds: nitrocyclobutane; nitrocyclopentane; nitro-cyclohexane; 1,2-dinitro cyclohexane; 1,3-dinitro cyclohexane; 1,4-dinitro cyclohexane and bis-(nitrocyclo-hexyl)-methanes.
The following are examples of suitable nitro alkanes: nitromethane, nitroethane, l-nitropropane;
2-nitropropane; nitrobutanes; nitropentanes; nitro-hexanes; nitrodecanes nitrocetanes; 1,2-dinitroethane, 1,2-dinitropropane; 1,3-dinitropropane; dinitrobutanes;
dinitropentanes; dinitrohexanes; dinitrodecanes; phenyl-nitromethane; bis-~nitromethyl)-cyclohexanes; bis-(nitromethyl)-benzenes and ~-nitro carboxylic acid nitriles.
Aromatic nitro compounds of the type exemplified above are preferred for the instant process. The following are particularly preferred: nitrobenzene;
1,3-dinitrobenzene; 2,4-dinitrobenzene; 2,6-dinitro-toluene and l,S-dinitronaphthalene.
The catalyst systems used for the instant process comprise: a) noble metals of the eighth subgroup of the periodic system as their main constituent and b) a cocatalyst component.
Components a) are either free noble metals of LeA 19,484 ~1334~
--ll--the eighth subgroup of the periodic system or compounds of these metals soluble in the reaction mixture. The noble metals are most preferably added as compounds which are soluble in the reaction mixture, for example, as chlorides, bromides, iodides, chloro complexes, bromo complexes, iodo complexes, acetates, acetyl acetonates and o,her soluble noble metal compounds.
Suitable noble metals include Ru, Rh, Pd, Os, Ir and Pt.
The preferred noble metals are palladium and rhodium, palladium being particularly preferred. Especially particularly preferred is palladium in the form of soluble palladium chloride. The preferred concentrations, based on the -eaction mixture including any soivent added, are generally in the range of 0.0001 to 0.1% by weight, in particular 0.001 to 0.01~ by weight, calculated as noble metal. If lower concentrations of noble metal are used, the reaction speed is too slow. Although higher noble metal concentrations could be used, this is uneconomical owing to the possible loss of noble metal, especially since any fu~ther increase in concentration does not increase the urethane yield.
The cocatalysts b) may be any compounds capable of Redox reactions under the reaction conditions of elements from the third to fifth main and first to eighth subgroup of the periodic system other than the compounds of group (a), The compounds of these metals are preferably their chlorides, oxychlorides, oxides and/or hydroxides. If oxides or hydroxides are used, certain activating chlorides are preferably also added.
The following are examples of suitable co-catalysts: copper(II)chloride; thallium(III)chloride;
tin(II)chloride; tin(IV)chloride; arsenic(III)chloride;
bismuth(III)chloride; vanadium(III)chloride; chromium LeA 19,484 (III)chloride; molybdenum(IVjchloride; tungsten(V) chloride; tungsten(VI)chloride; manganese~II)chloride;
iron(II)chloride; iron(III)chloride iron oxychloride;
cobalt(II)chloride; copper(II)oxide; copper(II)hydroxide;
thallium(I)hydroxide; tin(II)oxide; tin(II)hydroxide;
vanadium pentoxide; molybdenum trioxide; tungsten trioxide; manganese dioxide; iron(II)oxide; iron(II) hydroxide and iron(III)hydroxide. Also suitable are the iron(III)oxides, such as, for example, ~-Fe2O3 or y-Fe2O3; hydrated iron(III)oxides such as, for example, ~-FeO-OH; ~-FeO-OH or y-FeO-OH and iron spinel Fe3O4.
The particularly preferred cocatalysts include iron(II)chloride, iron(III)chloride, iron oxychloride and the oxides and hydrated oxides of trivalent iron.
The oxides or hydroxides exemplified above are often completely inert under the reaction conditions.
It is necessary in these cases, therefore, to use activating chlorides. These activating chlorides are compounds which contain anionically bound chlorine in the form of chloride and which are capable of reacting under the reaction conditions with the exemplified oxides or hydroxides to convert them at least partly into the corresponding chlorides or oxychlorides.
Suitable activating chlorides include, for example, the hydrochlorides of tertiary amines with molecular weights ranging from 59 to 300. Hydrochlorides of primary amines in which the substituents are preferably the same as the su~stituents of the ureas used, for example, aniline hydrochloride when diphenyl urea is used are also sultable. Hydrogen chloride, iron(II)chloride and iron(II)chloride complexes are more examples of suitable chloride compounds. The following are particularly suitable: pyridine LeA 19,4~4 1~33009 hydrochloride; aniline hydrochloride, the hydrochloride of 2,4-diamino toluene, hydrogen chloride, iron(II) chloride and complexes of iron(II)chloride. Combina-tions of the last mentioned compounds are particularly preferred. Activating chlorides with oxides and hydrated oxides of trivalent iron are particularly valuable cocatalysts.
The concentrations at which the cocatalysts including the activating chlorides are used in the instant process are generally from 0.1 to 20% by weight, preferably from 1 to 5~ by weight, based on the reaction mixture including any solvents used. If any activating chlorides are required, they are generally used in proportions of 0.05 to 10% by weight, pre-ferably from 0.1 to 2.5% by weight.
The reaction may be carried out in the presenceor absence of a solvent. The organic hydroxyl compound preferably used in excess generally serves as solvent.
Inert solvents may also be added in quantities of up to 80% by weight based on the whole reaction mixture.
Regardless of whether the solvent used is a hydroxyl compound used in excess or an inert solvent, its quantity must be such that the heat of reaction of exothermic urethane formation can be removed without any undue rise in temperature. The instant process is, therefore, generally carried out using a concentra-tion of urea compounds of from 5 to 50% by weight, preferably from S to 20% by weight, and organic nitro compounds as oxidizing agents at a concentration of from 1 to 20% by weight, preferably from 5 to 10% by weight, based on the whole reaction mixture including the solvent.
The solvents used should be inert towards the ~eA 19,484 reactants and the catalyst system. Examples are aromatic, cycloaliphatic and aliphatic hydrocarbons which may be substituted by halogen, such as benzene, toluene, xylene, chlorobenzene, dichlorobenzene, trichlorobenzene, chloro-naphthalene, cyclohexane, methyl cyclohexane, chloro-cyclohexane, methylene chloride, carbon tetrachloride, tetrachloroethane, trichlorotrifluoro ethane and similar compounds.
The reaction temperature generally ranges from 100C to about 300DC, in particular from 130C to 250C and most preferably from 140C to 220~C. The pressure must be calculated to ensure the continuous presence of a liquid phase and is generally in the range of 5 to 500 bar, most preferably from 30 to 300 bar at the reaction temperature. The reaction time required for quantitative conversion varies from a few minutes to several hours, according to the primary amine and hydroxyl compound used and any organic nitro compound present.
The reaction of the ureas with hydroxyl compounds, carbon monoxide and oxidizing agent to form urethanes may be carried out batchwise or continuously.
The batchwise reaction may be carried out in a high pressure autoclave with small quantities of homo-geneously dissolved noble metal and a sufficient excess of catalyst, and in the pr~sence of an activating chloride, if necessary. Compounds which are insoluble in the reaction medium, such as iron oxides or hydrated iron oxides, may be added in the form of a fine powder.
The activating additives may be added in the form of a homogeneous alcoholic solution. Undissolved excess cocatalyst components may be distributed by vigorous stirring of the reaction mixture or circulation by pumps.

LeA 19,484 1~33009 The exothermic heat of reaction may be removed by internally installed cooling apparatus or, if the reaction mixture is circulated by pumps, it may be removed by an external heat exchanger. Working up
5 of the reaction product and return of ihe catalyst may be carried out by various methods, according to the solubility of the resulting urethane in the reaction mixture. If the urethanes are readily soluble, for example, the major portion of the co-catalyst mixture which is only sparingly soluble atlow temperatures may be removed from the reaction product together with the major portion of absorbed palladium and organic amine salt, for example, by filtration or centrifuging. These compounds may be used again for a fresh reaction of primary amines with hydroxyl compounds, carbon monoxide and oxidizing agent. The liquid reaction mixture may be separated into solvents, pure urethanes and small quantities of by-products, if any, by the usual methods, e.g. by fractional distillation, either intermittently or continuously. The distillation residue contains small quantities of cocatalyst constituents dissolved in the reaction mixture and/or traces of noble metal and/or noble metal compounds. These substances may be returned for use in a fresh reaction.
If the urethanes are only soluble in the solvent or in excess hydroxyl compound, a modified method may be employed for wor~ing up the reaction mixture. For example, after release of pressure, the major portion of catalyst may be removed by filtration or centrifuging at a pressure and elevated temperature at which the urethanes are still dissolved but most of the catalyst system of noble metal/cocatalyst mixture precipitates.

LeA 19,484 The sparingly soluble urethane, possibly together with small auantities of sparingly soluble by-products and residues of catalyst, may then be crystallized by lowering the temperature. The mother liquor, which still contains small quantities of by-products, dissolved urethane and possibly dissolved cocatalyst constituents in addition to the solvent or excess organic hydroxyl compound used as solvent, may then either be directly returned to the reaction vessel, or the low boiling by-products contained in it may first be removed, for example, by distillation. Higher boiling by-products which cannot be removed by crystallization may be removed ccntinuously from the return stream as the distillation residue obtained from distilling an aliquot portion of the mother liquor.
The crude urethane precipitated may be recrystallized, for example, by crystallization from a solvent which dissolves the urethane at elevated temperatures but not the by-products and catalyst residues. Examples of such solvents include isooctane, benzene, toluene, xylene, chloro-benzene and dichlorobenzene. Those residues which are insoluble at elevated temperatures may be converted by oxidation into insoluble oxides such as, for example, iron oxides and an exhaust gas resulting from the organic impurities, which gas consists mainly of carbon dioxide, oxygen, nitrogen and possibly readily volatile organic impurities. The exhaust gas may, depending on its composition, either be directly discharged into the atmosphere or subjected to a catalytic afterburning to remove remaining impurities by oxidation. The oxidic compound obtained from the residue, which compound may still contain small quantities of noble metal and/or noble metal LeA 19,484 1~33009 compound, is returned to the oxycarbonylation process.
The reaction gas obtained from oxycarbonylation may contain unreacted carbon monoxide, low boiling organic consituents, small quantities of carbon S dioxide and also, if molecular oxygen was used as oxidizing agent, small quantities of unreacted oxygen, as well as the inert gas introduced, such as nitrogen.
This reaction gas may be readjusted to the reaction pressure after removal of the low boiling organic by-products and possibly carbon dioxide. It may then be returned to the reaction with replacement of the quantities of carbon monoxide and, if indicated, molecu-lar oxygen which have been used up.
The continuous reaction may be carried out in a cascade of reaction vessels, a system of reaction pipes, several reaction coils arranged one behind the other, an adiabatic reaction tube or several such tubes arranged one behind the other, or a bubble colu~n.
The heat may be removed either internally, for example, by the installation of cooling assemblies, or externally through a system of heat exchanger pipes, or adiabati-cally by the thermal capacity of the reaction mixture, followed by cooling in external cooling apparatus.
Subsequent working up may be carried out as described above, either continuously or discontinuously.
If the products of the instant process are used for their preferred purpose as intermediate products for the preparation of the corresponding isocyanates, it is often unnecessary to prepare them in the pure state and it may be sufficient to use the crude products obtained after filtering off the catalyst and, if indicated, distilling cff the solvent.
The following examples serve to il ustrate the process of the invention without restricting it in any LeA 19,484 way. In the Examples, all quantities quoted represent parts by weight or percent by weight, unless otherwise indicated.
EXAMPLES

250 g of a reaction mixture of the following composition were introduced into a 0.7 liter autoclave:
_~
2 x 10 '% by weight of palladium chloride, 3.7% by weight of iron oxychloride, 18.5% by weight of N,N'-diphenyl urea and 77.8% by weight of ethanol. 100 bar of carbon monoxide and 20 bar of air were forced in at room temperature. The mixture was allowed to react for one hour at 180~C. Gas chromatographic analysis of the liquid reaction product revealed 98% conversion of the diphenyl urea introduced into the process and aphenyl urethane selectivity of 72%, based on diphenyl urea, and of 98~, based on the reacted ethanol.

.
The same reaction mixture was used as in Example 1 but reacted twice, each time with 100 bar of carbon monoxide and 20 bar of air for one hour, so that the total reaction time was two hours at 180C. The diphenyl urea conversion was 99% and the phenyl urethane selectivities were: 88~ based on diphenyl 25 urea and 98 % based on ethanol.

The procedure was the same as in Example 1. A
mixture of ~-Fe2O3 (2.4% by weight) and aniline hydrochloride (3~ by weight) was used as cocatalyst.
Diphenyl urea conversion was quantitative and 80 mol ~
of phenyl urethane, based on diphenyl urea, and 98 mol %
thereof, based on reacted ethanol, were obtained.

LeA 19,484 1~330~

~ he following table gives the results or the reactions obtained when various cocatalysts based on oxide and activating chloride were used. 250 g of a mixture of the following composition were used in each case in a 0.7 liter autoclave: 1.7 x 10 3% by weight of PdC12, 2.4% by weight of an oxide capable of a Redox reaction, 3% by weight of aniline hydrochloride, 13.5% by weight of N,N'-diphenyl urea and 81.1~ by weight of ethanol. In each experiment, the mixture was reacted three times with 100 bar of carbon monoxide and 20 bar of air (at room te.mperature), each time for one hour at 180C (total reaction time - 3 hours at 180C in each experiment). The results shown in the following table were obtained:
~ Phenyl Urethane Example CocatalystDiphenyl UreaSelectivity Number OxideConversion % Urea Ethanol 4 V25 99 93 84.4 MnO2 100 90 99.3
6 MoO3 100 85 77
7 WO3 99 82.4 94.1
8 2 3 87.4 250 g of a reaction mixture of the following composition were introduced into a 0.7 liter refined steel autoclave: 2 x 10 3 by weight of PdC12, 4% by weight of iron oxychloride, 20% by weight of a mixture of N,N'-diphenyl urea and nitrobenzene in a molar ratio of diphenyl urea/nitrobenzene = 2:1 and 76% by weight of ethanol. 120 bar of monoxide were forced in at room temperature and the mixture was reacted for one hour at 160C. Gas chromatographic analysis showed quantitative LeA 19,484 ~33wg conversion of the diphenyl urea and the formation of phenyl urethane with a selectivity of 96%, based on diphenyl urea and nitrobenzene, and of 93% based on ethanol.

.
The follcwing Examples illustrate the influence of other noble metals on oxycarbonylation of N,N'-diphenyl urea (DPH) with nitrobenzene (NB):
Conditions:
10 Cocatalyst 3.7% by weight of iron oxy-chloride Diphenyl urea: 14.93~ by weight Nitrobenzene: 4.33~ by weight Molar ratio of diphenyl urea to nitrobenzene: 2:1 Alcohol: 77% by weight of ethanol Carbon monoxide pressure: 120 bar at 20C
Quantity of reaction mixture used: 270 g (in 0.7 liter refined steel autoclave) Results:
Noble Metal ExampleCompound Temperature Time Conversion %
Number(% by wei~ht) ~C Hrs. DPH NB
10RhCl (2.7 x 150 2 89 100 3 10-3) 11RhCl (2.7 x 180 1 99 100 3 10-3) 123 10-3) 180 1 99 100 134 10-3) lgO 2 99 100 14~uCl (3.7 x 180 2 99 100 LeA 19,484 Results (continued) Example Phenyl Urethane Selectivity ~
Number Based on DPH + NB Ethanol The following Examples illustrate the influence of the cocatalyst on oxycarboxylation of N,N'-diphenyl urea (DPH) with nitrobenzene(NB).
Conditions:
Noble metal: 1.8 x 10 3% by weight of PdC12 DPH + NB: 20~ by weight (in ethanol) Molar ratio N~H = 1.5:1 CO pressure: 120 bar at 20C
Temperature: 180C
Reaction time 1 h Reaction mixture: 270 g (in 0.7 liter refined steel autoclave) Results:

LeA 19,484 ~13300g ~ ~ ~ Phenyl Urethanë ' Selectivity %
Example Cocatalyst Conversion % Based On Number~% by weight) DPHNB DPH + NB Ethanol FeOCl (3.7) 99 100 96 96 16 FeC13 (3.6) 99 100 90 90 17 FeC12x4H2O 99 100 82 97 (5.5) lS VC13 (1.9) 99 100 92 94 19 CuC12 (1.9)+ 98 37 70 97 CeC13 (1.5) -Fe2O3 (2.5)~ 99 90 98 99.5 aniline .HCl (3.3) 21 V2o5 (2.5) + 99 100 93 100 aniline . HCl (3.3) 22 MoO3 (2.5) + 98 100 100 94 aniline .HCl (3.3) _XAMPLE 23 250 g of the following mixture were introduced into a 0.7 liter autoclave: 2 x 10 3% by weight of PdC12, 4~ by weight of FeOCl, 14.8% by weight of a bis-urea of 2,4-diamino toluene and 2-amino-4-nitrotoluene and 81% by weight of ethanol. The nitro groups of the urea used are oxidizing agents for the oxycarbonylation of the urea function. 120 bar of carbon monoxide were forced in at room temperature. The mixture was allowed to react for two hours at 180~C. The bis-urea was converted quantitatively. The bis-urethane of 2,4-diisocyanatotoluene was obtained with a selectivity of 50 mol % in addition to 10 mol~of isomeric amino-urethanes.
LeA 19,484

Claims (9)

The embodiments of the invention in which an exclusive pro-perty or privilege is claimed are defined as follows:
1. A process for the preparation of urethanes com-prising reacting N,N'-disubstituted ureas with organic compounds containing at least one hydroxyl group and oxycarbonylation in the presence of carbon monoxide and molecular oxygen and/or organic nitro compounds as oxidizing agents and a catalyst comprising:
(a) a noble metal and/or a noble metal compound of the eighth subgroup of the periodic system of elements, and (b) a compound capable of undergoing Redox reactions under the reaction conditions, of an element of the third to fifth main group and/or first to eighth subgroup of the periodic system of elements other than a compound of group (a).
2. A process as claimed in claim 1, wherein said N,N'-disubstituted ureas are symmetric N,N'-diaryl ureas and said nitro compound used is an aromatic nitro com-pound having the same aryl group as said urea.
3. A process for the preparation of urethanes comprising reacting nitro-substituted N,N'-diaryl ureas with organic compounds containing at least one hydroxyl group in the presence of carbon monoxide and, optionally, molecular oxygen with a catalyst comprising:
(a) a noble metal and/or a noble metal compound of the eighth subgroup of the periodic system of elements, and (b) a compound capable of undergoing Redox reactions under the reaction conditions, of an element of the third to fifth main group and/or first to eighth subgroup of the periodic system of elements other than a compound of group (a).
4. A process as claimed in claims 1 or 3, wherein said catalyst component (a) is palladium, rhodium, palladium compounds and/or rhodium compounds.
5. A process as claimed in Claims 1 or 3 wherein said catalyst components (b) are oxychlorides of elements of the third to fifth main group or first to eighth subgroup of the periodic system.
6. A process as claimed in Claims 1 or 3 wherein said catalyst components (b) are oxides and/or hydroxides of elements of the third to fifth main group or first to eighth subgroup of the periodic system in combination with compounds containing chlorine bound anionically as chloride characterized in that said chlorine compounds are capable of activating said oxides and/or hydroxides with formation of chloride.
7. A process as claimed in Claims 1 or 3 wherein said catalyst component (b) is iron oxychloride.
8. A process as claimed in Claims 1 or 3 wherein said organic compounds having at least one hydroxyl group are monohydric primary aliphatic alcohols having from 1 to 6 carbon atoms.
9. A process as claimed in Claims 1 or 3 wherein said reaction is carried out at a temperature of from 100 to 300°C and a pressure of from 5 to 500 bars.

LeA 19,484
CA345,675A 1979-03-02 1980-02-14 Process for the preparation of urethane Expired CA1133009A (en)